FGH95/MT-Ni95 Superalloy Rod

    Application: Roads, Railways, Bridges, Construction

     

    Type: Rotary

     

    Power Type: Electric

Shanghai Metal Corporation is a leading FGH95/MT-Ni95 Superalloy Rod manufacturer and supplier.

Our products have passed ISO9001、ISO13485、GJB9001C quality management system and stand the end users’ ordeal. We devote ourselves to manufacture the high-quality products with competitive prices, we know the industries well, therefore from design to material selection, till manufacturing technique is up to the high standard, meanwhile our planning team and international team will ensure the punctual delivery.

If you want to know more about our FGH95/MT-Ni95 Superalloy Rod price please feel free to contact us, we will reply you within 24 hours.


Technical Information of FGH95/MT-Ni95 Superalloy Rod:

 

C (%)

Si (%)

Mn (%)

P (%)

S (%)

Cr (%)

Ni (%)

Mo (%)

W (%)

Co (%)

B (%)

Nb (%)

Al (%)

Ti (%)

Ta (%)

Fe (%)

0.04-0.09

0.2

0.15

0.015

0.015

12.00-14.00

Bal

3.30-3.70

3.30-3.70

7.00-9.00

0.006-0.015

3.30-3.70

3.30-3.70

2.30-2.70

≤0.020

≤0.50

 

Mechanical Properties of steel grade FGH95 

Yield Strength Rₚ₀.₂ (MPa) 

Tensile Strength Rₘ (MPa) 

Impact Value KV/Ku (J)

Elongation A (%)

Reduction in Cross Section on Fracture Z (%)

Brinell Hardness HBW

≥495

≥881

22

41

41

334

Packaging of FGH95/MT-Ni95 Superalloy Rod:

 

Package Type: Plastic Bag + Carton + Wooden case

Products & Service
Click here for price
Click
here
for
price
* E-mail
* Country
* Company name
WhatsApp
Tel

Home

Search

Inquiry

Top